Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 7.60 g/micron
193 g/mil
ISO 6383-2
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film
LDPE 1022 FN 24 is a low density polyethylene made by a high pressure process without antioxidant.LDPE 1022 FN 24 is suited to many applications in the field of consumer, industrial, food or hygiene..