Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | >= 0.512 g/micron | >= 13.0 g/mil | ASTM D1922 |
NIZHNEKAMSKNEFTEKHIM PE 4148B (484H2) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Elmendorf Tear Strength, MD | >= 0.512 g/micron | >= 13.0 g/mil | ASTM D1922 |
NIZHNEKAMSKNEFTEKHIM PE 6152C (526H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Elmendorf Tear Strength, MD | 0.512 g/micron | 13.0 g/mil | ASTM D1922 |
Formosa Plastics Formolene® E905 Film HDPE
(discontinued **) HMW-Bimodal ResinApplications: T-shirt bags, trash can liners, heavy duty bagsFormolene E905 is a high molecular weight grade of HDPE with well-balanced strength in both the machine (MD) and transve.. |
|||
Elmendorf Tear Strength, MD | 0.512 g/micron | 13.0 g/mil | Notched; ASTM D1922 |
Chevron Phillips MarFlex® 9656 HDPE Blown Film Resin Resin Type: high density, linear polyethylene.Characteristics: copolymerization enhances film toughness, good drawdown, density level gives good machinability, blend well with LLDPEApplications: not.. |