Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 9.25 g/micron | 235 g/mil | ASTM D1922 |
ExxonMobil Exceed™ 1023CA Tough Premium Film Resin
(discontinued **) Exceed 1023CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023CA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Elmendorf Tear Strength, MD | 9.25 g/micron | 235 g/mil | ASTM D1922 |
Dow AFFINITY™ PF 1140G Polyolefin Plastomer (POP) AFFINITY™ PF 1140G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to be used in a variety of demanding applications including form-fill-seal packaging and fre.. |