Polymer Property : Elmendorf Tear Strength, MD = 5.60 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 5.60 g/micron
142 g/mil
Reliance Industries LLDPE film - Organic acid based film
Information provided by Reliance Industries
Elmendorf Tear Strength, MD 5.60 g/micron
142 g/mil
ASTM D1922
NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin  (discontinued **)
Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi..
Elmendorf Tear Strength, MD 5.60 g/micron
142 g/mil
ISO 6383-2
Total LLDPE LL 1820 H Linear Low Density Polyethylene - Blown Film
LL 1820 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 H can be processed at high o..
Elmendorf Tear Strength, MD 5.60 g/micron
142 g/mil
ISO 6383-2
Total LLDPE LL 1820 Linear Low Density Polyethylene - Blown Film
LL 1820 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 can be processed at high outpu..
Elmendorf Tear Strength, MD 5.60 g/micron
142 g/mil
ASTM D1922
Total Lotrene® Q2018C Linear Low Density Polyethylene, Blown Film
Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form ..
Elmendorf Tear Strength, MD 5.60 g/micron
142 g/mil
ASTM D1922
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film
Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form ..
Elmendorf Tear Strength, MD 5.60 g/micron
142 g/mil
ASTM D1922
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film
Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form ..
Elmendorf Tear Strength, MD 5.60 g/micron
142 g/mil
ASTM-D1922
Braskem LL6802N LLDPE Blown Film Extrusion Polyethylene Copolymer
LL6802N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing aid ..
Elmendorf Tear Strength, MD 5.60 g/micron
142 g/mil
ASTM-D1922
Braskem TS9002 LDPE Blown Film Extrusion Polyethylene
TS9022 is a low-density polyethylene (LDPE) developed specially for automatic overwrap packaging. This resin has a combination of high optical properties and excellent stiffness. The incorporated ad..
Elmendorf Tear Strength, MD 5.60 - 24.0 g/micron
142 - 610 g/mil
Average value: 14.2 g/micron Grade Count:34
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum..