Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 5.10 g/micron | 130 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® PF-Y821-BP Butene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, intended for narrow die gaps.Applications: General purpose packaging, bags requiring moderate clarity, bread bags.Data provided by the m.. |
|||
Elmendorf Tear Strength, MD | 5.10 g/micron | 130 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® PF-Y821-CP Butene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, suitable for narrow die gaps.Applications: Industrial packaging, heavy duty sacks.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, MD | 5.10 g/micron | 130 g/mil | ISO 6383-2 |
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film Lumicene® mPE M 2735 S01 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 2735 S01 can be processed at high output rates with low extrusion pressure, low nec.. |
|||
Elmendorf Tear Strength, MD | 5.10 g/micron | 130 g/mil | ASTM 1922 |
Braskem LL 118/21 LLDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem |