Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 10.7 g/micron | 271 g/mil | ASTM D1922 |
ExxonMobil Escorene® LL-3113 LLDPE/Hexene Premium High Strength, 0.7 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Elmendorf Tear Strength, MD | 10.7 g/micron | 273 g/mil | ASTM D1922 |
ExxonMobil Exceed™ 399L60 LDPE/Hexene Premium Blown Film Resin, 3 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 399L60 resin have balanced tensile, impact strength,.. |
|||
Elmendorf Tear Strength, MD | 10.7 g/micron | 272 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-334 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 4.2% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |