Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 6.21 MPa | 900 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 135.09 Cast Packaging Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. It is suitable for processing in cast film equipment. Applications include food packaging, light to medium duty bags, and textile packaging.. |
|||
Film Tensile Strength at Yield, TD | 6.21 MPa | 900 psi | at 2% offset; ASTM D882 |
ExxonMobil Escorene® LD 712.06 Film Resin
(discontinued **) Escorene Ultra LD 712 series is a fraction melt index, 10 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particular.. |
|||
Film Tensile Strength at Yield, TD | 6.21 - 15.9 MPa | 900 - 2300 psi | Average value: 10.9 MPa Grade Count:140 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |