Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | ASTM D882 |
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 135.09 Blown Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. Applications include food packaging, light to medium duty bags, and textile packaging.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | |
Dow LDPE 501I Low Density Polyethylene, Clear Film Grade DOW LDPE 501I, a barefoot resin used for bakery film and other packaging applications that require optical clarity. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food con.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | |
Dow LDPE 503A Low Density Polyethylene, Liner Film Grade DOW LDPE 503A resin is used for liner film and other packaging applications that require optical clarity. It contains medium levels of slip additive and low levels of antiblock additive. It complies.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | |
Dow LDPE 640I Low Density Polyethylene, Liner Film Grade DOW LDPE 640I resin is a barefoot general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. This material complies with U.S.FDA regulation 21 CFR .. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | |
Dow LDPE 641I Low Density Polyethylene, Liner Film Grade DOW LDPE 641I resin is a general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. It contains medium levels of slip additive and low levels of an.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | |
Dow LDPE 682I Low Density Polyethylene, Film Grade DOW LDPE 682I barefoot resin is used for shrink, frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. T.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | |
Dow LDPE 683I Low Density Polyethylene, Film Grade DOW LDPE 683I resin is a general purpose resin with low levels of antiblock additive used for frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | ASTM D882 |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |