Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 453 Polyester Film, 300 Gauge Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 453 Polyester Film, 400 Gauge Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 453 Polyester Film, 500 Gauge Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 453 Polyester Film, 700 Gauge Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 200 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 400 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 500 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 700 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 92 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 455 Polyester Film Melinex® 455 is a high clarity polyester film pretreated on one side for slip. It has excellent handling characteristics.General Product Info: Two smooth coatable surfacesLow surface resistivityCan.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 456 Polyester Film Melinex® 456 is an excellent handling, high clarity polyester film with both sides pretreated for slip. The two smooth surfaces allow easy top coating.Approvals: UL 94 VTM-2 - for 200 - 700 gauge (.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 561 Polyester Film Melinex® 561 is a high clarity polyester film which is pretreated on both sides to promote adhesion to many industrial coatings and inks. Melinex® 561 is suitable for applications which require a .. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 595 Polyester Film, 400 Gauge Melinex® 595 is a high clarity film that is one side pretreated to provide anti-charge protection and one side pretreated to promote adhesion to many solvent coating formulations. This film is exce.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 965 Polyester Film, 500 Gauge Melinex® 965 is a slightly hazy film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems. It has a superb web handleability.Information provided by.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 966 Polyester Film, 700 Gauge Melinex® 966 is a slightly hazy film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems. It has a superb web handleability.Information provided by.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® WCW Polyester Film, 200 Gauge Melinex® WCW is a translucent white polyester film with a rough surface for superior handling characteristics.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® WCW Polyester Film, 75 Gauge Melinex® WCW is a translucent white polyester film with a rough surface for superior handling characteristics.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 142 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 275 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 400 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 500 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 650 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 6428 Polyester Film, 200 Gauge Melinex® 6428 is a high clarity polyester film. It is pretreated on both film surfaces to promote adhesion to EVA. Melinex® 6428 is a developmental film designed for the photovoltaics industry.Als.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 943 Polyester Film Melinex® 943 is a super clear film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® HS2 Polyester Film Melinex® HS2 is a low TD shrinkage, low neckdown polyester film with excellent handling properties. It is ideal for the hot stamping marketInformation provided by DuPont. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa @Strain 5.00 % |
14000 psi @Strain 5.00 % |
ASTM D882 |
DuPont Teijin Films Mylar® A Polyester Film, 92 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 92 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LJP Polyester Film, 200 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 142 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Yield, TD | 96.5 MPa | 14000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 300 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |