Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 7.10 MPa | 1030 psi | ASTM D882 |
ExxonMobil Exceed™ 357C32 LDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 357C32 resin have outstanding tensile properties and.. |
|||
Film Tensile Strength at Yield, TD | 7.10 MPa | 1030 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 307.76 Clear, High Impact Film Resin LD 307.76 film has superior impact strength and heat sealability, used in frozen and other food packaging, and high strength bags.Information provided by ExxonMobil Chemical |