Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Resistance | 0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
cond; ISO 180/1A |
DSM Stanyl® TS300 PA46 |
|||
Izod Impact Resistance | 0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
dry; ISO 180/1A |
DSM Stanyl® TS300 PA46 |
|||
Izod Impact Resistance | 0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
dry; ISO 180/1A |
DSM Stanyl® TW242FM10 PA46-(GF+MF)50 50% Glass/Mineral Reinforced, Heat Stabilized |
|||
Izod Impact Resistance | 0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
cond; ISO 180/1A |
DSM Stanyl® TW341-B PA46 Heat Stabilized, Lubricated |
|||
Izod Impact Resistance | 0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
dry; ISO 180/1A |
DSM Stanyl® TW341-B PA46 Heat Stabilized, Lubricated |
|||
Izod Impact Resistance | 0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
cond; ISO 180/1A |
DSM Stanyl® TW341-J PA46 Heat Stabilized, Lubricated |
|||
Izod Impact Resistance | 0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
dry; ISO 180/1A |
DSM Stanyl® TW341-J PA46 Heat Stabilized, Lubricated |
|||
Izod Impact Resistance | 0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
cond; ISO 180/1A |
DSM Stanyl® TW341-N PA46 Heat Stabilized, Lubricated |
|||
Izod Impact Resistance | 0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
dry; ISO 180/1A |
DSM Stanyl® TW341-N PA46 Heat Stabilized, Lubricated |
|||
Izod Impact Resistance | 0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
cond; ISO 180/1A |
DSM Stanyl® TE300 PA46 Heat Stabilized |
|||
Izod Impact Resistance | 0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
dry; ISO 180/1A |
DSM Stanyl® TE300 PA46 Heat Stabilized |