Polymer Property : Torsional Stiffness = 135000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Torsional Stiffness 930 MPa

@Temperature <=-70.0 °C
135000 psi

@Temperature <=-94.0 °F
ASTM D1043
Eastman Eastman AP005 Copolyester
Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly..
Torsional Stiffness 930 MPa

@Temperature <=-70.0 °C
135000 psi

@Temperature <=-94.0 °F
ASTM D1043
Eastman Eastman AP006 Copolyester
Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly..
Torsional Stiffness 930 MPa

@Temperature <=-70.0 °C
135000 psi

@Temperature <=-94.0 °F
ASTM D1043
Eastman Eastman AP007 Copolyester
Applications:Automotive componentsBreathable filmsElectronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsOffice furniturePackagingPolymer modificationProfilesRubber an..