Polymer Property : Shear Modulus = 0.0971 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus >= 0.0971 GPa

@Temperature -50.0 - 250 °C
>= 14.1 ksi

@Temperature -58.0 - 482 °F
Average value: 0.632 GPa Grade Count:2
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..