Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Fastener Stock
Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of fastener stock; more specific form/thickness entries are also available in MatWeb.Industry Specifications: ..
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod
Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of rod; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aeros..
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness,
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness,
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness,
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness,
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G; other specific form/thickness entries ..
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet
Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of sheet; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aero..
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265; other specific form/thickness entries a..
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5),
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >0.500-1.000 in, STD, Per Mil-T-9047G
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >0.500-1.000 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i..
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >1.000-1.500 in, STD, Per Mil-T-9047G
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >1.000-1.500 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i..
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G; other specific form/thickness entries are ..
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET 6-4 Titanium Alloy (Ti-6Al-4V-0.1Ru; ASTM Grade 29)
Medium To High Strength General-Purpose Alloy. Property data below are typical of Timet® 6-4 ELI (without Ru). The 0.1 Ru ELI variant is used for enhanced corrosion resistance.Data provided by TI..
Shear Modulus 43.0 - 45.0 GPa
6240 - 6530 ksi
TIMET TIMETAL® 3-2.5 -0.05Pd Titanium Alloy
Cold Workable Medium Strength Alloy. Palladium is added to this grade to enhance its corrosion behavior. Property data below is typical of TIMETAL® 3-2.5 Titanium Alloy.Data provided by TIMET.
Shear Modulus 43.0 - 45.0 GPa
6240 - 6530 ksi
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Aged
Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to aged material; other specific condition entries are also available in MatWeb.Features: Cold formable and we..
Shear Modulus 43.0 - 45.0 GPa
6240 - 6530 ksi
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Annealed
Cold Workable Medium Strength Alloy. UTS, TYS, Elongation, R.A. and bend radius data below are specific to annealed material; other specific condition entries are also available in MatWeb.Features..
Shear Modulus 43.0 - 45.0 GPa
6240 - 6530 ksi
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Typical Properties
Cold Workable Medium Strength AlloyFeatures: Cold formable and weldable, this alloy is used primarily for honeycomb foil and hydraulic tubing applications. Industrial applications such as pressure v..
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed;
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A..
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed;
Medium To High Strength General-Purpose Alloy Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A ..
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 1.75 - 2.50 in Rod or Thickness; Per ASTM F136)
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A..
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 2.50 - 4.00 in Rod or Thickness; Per ASTM F136)
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A..
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Solution Treated; 0.025 - 1.000 in Sheet and Plate; Per ASTM B265)
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A..
Shear Modulus 41.0 - 45.0 GPa
5950 - 6530 ksi
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Rod, Square, or Hex, >1.500-2.000 in, Per Mil-T-9047G
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod, Square, or Hex, >1.500-2.000 in, Per Mil-T-9047G; other specific form/thickness entries are ..
Shear Modulus 43.0 - 45.0 GPa
6240 - 6530 ksi
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) CWSR
Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to CWSR condition; other specific condition entries are also available in MatWeb.Features: Cold formable and w..