Shear Modulus 0.0430 GPa

@Temperature -12.0 °C
6.24 ksi

@Temperature 10.4 °F
ASTM D1053
Precision Polymer Engineering V70D Fluoroelastomer Compound
Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Meets Aerospace Specifications DTD5612A and DTD5543B Grade 70.Applications: Mouldings which are requ..
Shear Modulus 0.0430 GPa

@Temperature -12.0 °C
6.24 ksi

@Temperature 10.4 °F
ASTM D1053
Precision Polymer Engineering V75B Fluoroelastomer Compound
Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M2HK710, A1-10, B37, B38, EF31, EO78, F14, Z1, where Z1 = compressi..
Shear Modulus 0.0430 - 0.0430 GPa

@Temperature -12.0 - -12.0 °C
6.24 - 6.24 ksi

@Temperature 10.4 - 10.4 °F
Average value: 0.0430 GPa Grade Count:2
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..