Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Modulus = 4210 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 29.0 GPa
4210 ksi
calculated
Piezo Kinetics 402 Lead Zirconate Titanate Piezoelectric
Denoted as Navy Type I, it is designed to serve as a driver where high power and low losses are dictated by design. It is primarily well suited for ultrasonic cleaners and sonars.Elastic Compliance ..
Shear Modulus 29.0 GPa
4210 ksi
calculated
Piezo Kinetics 409E Lead Zirconate Titanate Piezoelectric
Denoted as Navy Type I, it is designed to serve as a driver where high power and low losses are dictated by design. It is primarily well suited for ultrasonic cleaners and sonars.Elastic Compliance ..
Shear Modulus 29.0 GPa
4210 ksi
calculated
Piezo Kinetics 804 Lead Zirconate Titanate Piezoelectric
Denoted as Navy Type III, it is specifically used as a driver that exhibits low losses under extreme driving conditions and has a high Q. PKI 804 is well suited for medical applications.Elastic Comp..
Shear Modulus 29.0 GPa
4210 ksi
calculated
Schott N-BAK1 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 29.0 GPa
4210 ksi
calculated
Schott N-BAK2 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 29.0 GPa
4210 ksi
calculated
Schott N-K5 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 29.0 GPa
4210 ksi
calculated
Schott N-PK51 Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
Shear Modulus 29.0 GPa
4210 ksi
calculated
Schott N-ZK7 Glass
Information Provided by SCHOTT North America, Inc.
Copyright © lookpolymers.com All Rights Reserved