Mechanical Properties Metric English Comments
Shear Modulus >= 0.0180 GPa
>= 2.61 ksi
ASTM C393
3A Composites Core Materials AIREX® R63.80 Damage Tolerant Foam
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable..
Shear Modulus 0.0180 GPa
2.61 ksi
average; ASTM C393
3A Composites Core Materials AIREX® R82.60 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver..
Shear Modulus >= 0.0180 GPa
>= 2.61 ksi
ASTM C393
3A Composites Core Materials AIREX® T92.100 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..
Shear Modulus >= 0.0180 GPa
>= 2.61 ksi
ASTM C393
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..
Shear Modulus >= 0.0180 GPa
>= 2.61 ksi
ASTM C393
3A Composites Core Materials AIREX® C70.55 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..
Shear Modulus >= 0.0180 GPa
>= 2.61 ksi
ASTM C393
3A Composites Core Materials AIREX® C71.55 Elevated Temperature Structural Foam
AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength..