Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 77.4 GPa | 11200 ksi | Calculated |
Latrobe LSSâ„¢ 17-4 Precipitation Hardening Stainless Steel (ASTM Type 360) TLS 17-4 is a precipitation hardening, martensitic stainless steel that exhibits excellent resistance to atmospheric and chemical corrosion. TLS 17-4 exhibits an excellent combination of high stren.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip General Elgiloy® information: High strength, ductility, fatigue life, and good mechanical properties. Corrosion resistant in numerous environments. Available in strip (currently 0.0015" to 0.075".. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 10% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 20% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 20% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 30% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 40% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 40% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 65% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 65% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, Heat Treated Heat Treatment 5 hours at 482°C. The strength and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, duc.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 10% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 30% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, Heat Treated Heat Treatment 5 hours at 527°C. The strength and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, duc.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | Calculated |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1100 (Heated 593°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | Calculated |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Annealed Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | Calculated |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1075 (Heated 579°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | Calculated |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150 (Heated 621°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | Calculated |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150M (Heated 760°C/2hr/AC then 621°C/4hr/AC) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | Calculated |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | Calculated |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1025 (Heated 552°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Shear Modulus | 77.4 GPa | 11200 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Wire The strength and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fatigue life, and.. |