Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 3.00 - 5.00 GPa | 435 - 725 ksi | Average value: 3.83 GPa Grade Count:3 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Shear Modulus | 3.00 - 5.82 GPa | 435 - 844 ksi | Average value: 3.73 GPa Grade Count:14 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
Shear Modulus | 3.00 GPa | 435 ksi | Calculated |
Plenco 4485 Phenolic, Granular, Injection Molded PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a.. |
|||
Shear Modulus | 3.00 GPa | 435 ksi | Calculated |
Plenco 7100 Phenolic, Nodular, Injection Molded PLENCO 07100 is an organic fiber reinforced phenolic molding compound, with improved mechanical strength properties and an industrial finish. 07100 is densified for easy handling and good pourabilit.. |
|||
Shear Modulus | 3.00 GPa | 435 ksi | In-Plane, RT, Dry; EN6031 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 54%/G1088 Glass/Carbon Fiber Information provided by HexCel |
|||
Shear Modulus | 3.00 GPa | 435 ksi | Calculated |
Plenco 7307 Phenolic, Granular, Transfer Molded PLENCO 07307 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties. Type ASTM 5948 CFG, and UL recognized under component file E40654. 07307 is a.. |