Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 155 GPa | 22500 ksi | Calculated |
CoorsTek ADS-995 99.5% Alumina Thin Film Applications: thin film substrates |
|||
Shear Modulus | 155 GPa | 22500 ksi | Calculated |
CoorsTek ADS-996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Shear Modulus | 155 GPa | 22500 ksi | Calculated |
CoorsTek SC-DSLP (SC-50) Liquid Phase Sintered Silicon Carbide Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Shear Modulus | 155 GPa | 22500 ksi | Calculated |
CoorsTek Superstrate® 996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Shear Modulus | 155 GPa | 22500 ksi | Calculated |
CoorsTek Superstrate® TPS 99.6% Alumina Thin Film Applications: thin film substrates |