Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.35 - 1.46 GPa | 196 - 212 ksi | Calculated |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist.. |
|||
Shear Modulus | 1.35 GPa | 196 ksi | ISO 6721-2 |
Styrolution Polystyrol 143 E GR 2 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Shear Modulus | 1.35 GPa | 196 ksi | ISO 6721-2 |
Styrolution Polystyrol 143 E GR 21 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Shear Modulus | 1.35 GPa | 196 ksi | ISO 6721-2 |
Styrolution Polystyrol 145 D PS Description: Polystyrol 145 D is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol.Applications: In blends with high impact polystyrene esp.. |
|||
Shear Modulus | 1.35 GPa | 196 ksi | Calculated |
Hexcel® HexPly® 920 125°C Curing Epoxy Matrix HexPly® 920 is a very tough advanced resin matrix, ideally suited to the single-shot production of honeycomb sandwich structures and the manufacture of solid laminates. It is highly tolerant of a v.. |