Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.580 GPa | 84.1 ksi | DIN 53457 |
Global PP-2300-LC Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-furniture, crates, closures, electrical appliances, automotiveInformation provided by Global Polyme.. |
|||
Shear Modulus | 0.580 GPa | 84.1 ksi | DIN 53457 |
Global PP-3342-M Polypropylene Random Copolymer Description-medium stiffness, low melting temperatures, very good for seal Applications-housewares, cookwareInformation provided by Global Polymers Corporation. |