Polymer Property : Fracture Toughness = 3.64 ksi-in½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 3.00 - 4.00 MPa-m½
2.73 - 3.64 ksi-in½
Notched Beam
CoorsTek AD-85 Alumina (nom. 85% Al2O3)
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Fracture Toughness 3.00 - 4.00 MPa-m½
2.73 - 3.64 ksi-in½
Notched Beam
CoorsTek AD-90 Alumina (nom. 90% Al2O3)
Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Fracture Toughness 3.00 - 4.00 MPa-m½
2.73 - 3.64 ksi-in½
Klc; Notched Beam
CoorsTek ADD-96 96% Alumina
Fracture Toughness 3.00 - 4.00 MPa-m½
2.73 - 3.64 ksi-in½
Klc; Notched Beam
CoorsTek Boron Carbide Reaction-Bonded Boron Carbide
Lowest density for ultra-lightweight designs