Polymer Property : Fracture Toughness = 4.10 MPa-m½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 4.10 MPa-m½
3.73 ksi-in½
K<sub>IC</sub>; DIN 51109
CeramTec Rocar® ST Silicon Carbide, SSiC
Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. Its outstanding sliding properties and high thermal conductivity make useful in tribological applicat..
Fracture Toughness 4.10 MPa-m½
3.73 ksi-in½
Ceradyne CeraTrex™ 146-12E Silicon Carbide
Features:corrosion resistancewear resistancetailored electrical propertiesApplications:semiconductor componentsInformation provided by Ceradyne Company
Fracture Toughness 4.10 MPa-m½
3.73 ksi-in½
K<sub>IC</sub>
CeramTec Rubalit® A 1898 Alumina, 98%
Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond ..