Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.24 GPa | 905 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp RFZ42 PA 66 LNP* Thermocomp* RFZ42 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 6.24 GPa | 905 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp RFZ42 PA 66 (Asia Pacific) LNP* Thermocomp* RFZ42 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass.This data was supplied by SABIC-IP for the Asia Pacific region. |