Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0630 GPa | 9.14 ksi | ISO 527 |
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Modulus | 0.0630 GPa | 9.14 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide PF004EUC PA6, 20% Glass Filled, Injection Molded PF004EUC is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |