Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.14 GPa | 891 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF003AXH PA 66 LNP* THERMOCOMP* RF003AXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material includes: Healthcare. |