Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 57.0 GPa | 8270 ksi | |
Goodfellow Iron 78/Boron 13/Silicon 9 Alloy Information provided by Goodfellow. |
|||
Tensile Modulus | 57.0 GPa @Temperature 80.0 °C |
8270 ksi @Temperature 176 °F |
Tensile Warp, Wet; Pr EN 2561 |
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process. |
|||
Tensile Modulus | 57.0 GPa @Temperature 23.0 °C |
8270 ksi @Temperature 73.4 °F |
0°, Conditioning: 23°C; ASTM D3039 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, HTA Fiber Designation: C193PW, Plain weaveInformation provided by HexCel |
|||
Tensile Modulus | 57.0 GPa | 8270 ksi | 90º, RT, Dry; EN2561 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber Information provided by HexCel |