Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.21 GPa | 756 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RZ006S PA 66 LNP* THERMOCOMP* RZ006S is a compound based on Nylon 66 resin containing 30% Milled Glass. Added feature of this material is: Heat Stabilized. |
|||
Tensile Modulus | 5.21 GPa | 756 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RZ006S PA 66 (Asia Pacific) LNP* Thermocomp* RZ006S is a compound based on Nylon 66 resin containing Milled Glass. |
|||
Tensile Modulus | 5.21 GPa | 756 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP SF004S PA12 LNP* Thermocomp* SF004S is a compound based on Nylon 12 containing 20% glass fiber. Added features include: Heat Stabilized, Healthcare |