Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.97 GPa | 721 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF002XXH PA 66 LNP THERMOCOMP* RF002XXH is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
Tensile Modulus | 4.97 GPa | 721 ksi | 1 mm/min |
Arkema Group Rilsan® BMN Y BZ TL Nylon 11, Bronze Bead Filled (Dry) Designation ISO 1874-PA11,MHLS,16-020,(Z+M)(B+D)(80BZ+05)Rigid grade with bronze beads (85%) and molybdenum fillers for injection molding. Available color: steel brown. Light and heat stabilized.No .. |