Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.483 GPa | 70.0 ksi | 1% Secant; ASTM D638 |
LyondellBasell Purell® PE3220D Low Density Polyethylene, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding Purell PE 3220 D is a low density polyethylene with high rigidity and good chemical resistance. It is delivered in pellet form. Target markets are packaging of pharmaceuticals in the small blow mold.. |
|||
Tensile Modulus | 0.483 - 0.621 GPa | 70.0 - 90.0 ksi | |
ITW Plexus Plexusâ„¢ MA422 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, medium open time.Information provided by Illinois Tool Works. |
|||
Tensile Modulus | 0.483 GPa | 70.0 ksi | ASTM D-882 |
Saint-Gobain Norton® FEP Fluoropolymer Film Features/Benefits:Outstanding clarityOutstanding anti-stick release propertiesPerformance from -254°C (-425°F) to 205°C (400°F)Exceptional chemical resistance and electric propertiesComp.. |
|||
Tensile Modulus | 0.483 GPa | 70.0 ksi | ASTM D-882 |
Saint-Gobain Norton® PFA Fluoropolymer Film Features/Benefits:Outstanding flex life and stress crack resistancePerformance from -254°C (-425°F) to 260°C (500°F)Outstanding anti-stick release propertiesExcellent electrical properti.. |
|||
Tensile Modulus | 0.483 GPa | 70.0 ksi | at 1% Strain |
3M Scotch-Weld™ DP8010 Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl.. |
|||
Tensile Modulus | 0.483 GPa | 70.0 ksi | ASTM D638 |
Quadrant EPP Quicksilver® UHMW-PE Premium Truck Lining (ASTM Product Data Sheet) |
|||
Tensile Modulus | 0.483 - 0.621 GPa | 70.0 - 90.0 ksi | |
ITW Plexus Plexus™ MA922 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, medium open time.Information provided by Illinois Tool Works. |