Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.73 GPa | 686 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP SH1100A PA12 LNP* Thermocomp* SH1100A is a Nylon 12, High Specificy Gravity compound containing proprietary fillers. |
|||
Tensile Modulus | 4.73 GPa | 686 ksi | Storage |
Epoxy Technology EPO-TEK® EV2118-2 Silver-filled, electrically conductive epoxy Preliminary Product Information SheetMaterial Description: A silver-filled, electrically conductive epoxy designed for semiconductor and electronic assembly.Information Provided by Epoxy Technology |