Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.45 GPa | 645 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp DFP22 PC LNP* DFP22 is a Polycarbonate base resin containing glass fiber and PTFE/Silicone Lubricants. Characteristic of this grade is: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
Tensile Modulus | 4.45 GPa | 645 ksi | |
Henkel Hysol EA 934NA Paste Adhesive System Two part adhesive system with superior strengthCures at room temperatureApplications: Potting Structural Repair Liquid Shim |
|||
Tensile Modulus | 4.45 GPa | 645 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC STAMAX 20YK270 PP SABIC® STAMAX 20YK270 is a 20% long glass fiber reinforced polypropylene with improved impact and flow properties. The glass fibers are chemically coupled to the PP matrix, resulting in high stif.. |
|||
Tensile Modulus | 4.45 GPa | 645 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Tensile Modulus | 4.45 GPa | 645 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Tensile Modulus | 4.45 GPa | 645 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Tensile Modulus | 4.45 GPa | 645 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Tensile Modulus | 4.45 GPa | 645 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |