Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.415 GPa | 60.2 ksi | 1 mm/min |
Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA12-P,EHL,22-004Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Very good chemical.. |