Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.79 GPa | 550 ksi | TM R050-36 |
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy EP950G Gray is an aluminum filled one part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated temperature. It is a medium paste-like viscosi.. |
|||
Tensile Modulus | 3.79 GPa | 550 ksi | ASTM D638 |
Fiberfil® PP-60/TC/20/VO/ND Polypropylene Homopolymer, 20% Talc Filled, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 3.79 GPa | 550 ksi | ASTM D638 |
Ensinger Tecapeek® XP-95 Compression Molded PEEK Compound, 15% PTFE Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Modulus | 3.79 GPa | 550 ksi | ASTM D822 |
DuPont Teijin Films Mylar® CL Polyester Film, 100 Gauge Mylar® CL is an exceptionally strong polyester film designed to package foods. Foods can be heated or cooked in this film at temperatures up to 400°F. Mylar® CL is commercially available in nomin.. |
|||
Tensile Modulus | 3.79 GPa | 550 ksi | ASTM D882 |
DuPont Teijin Films Mylar® OB13AF Polyester Film, 100 Gauge Product Description: Mylar® OB13AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite s.. |
|||
Tensile Modulus | 3.79 GPa | 550 ksi | ASTM D882 |
DuPont Teijin Films Mylar® RL31 Polyester Film, 100 Gauge Mylar® RL31 is a biaxially oriented polyester (OPET) with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Myl.. |
|||
Tensile Modulus | 3.79 GPa | 550 ksi | ASTM D882 |
DuPont Teijin Films Mylar® RL31 Polyester Film, 50 Gauge Mylar® RL31 is a biaxially oriented polyester (OPET) with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Myl.. |
|||
Tensile Modulus | 3.79 - 5.17 GPa | 550 - 750 ksi | ASTM D638 |
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon Offering improved tensile, compressive and flexural properties over conventional unfilled cast nylon, NYCAST® GF (Glass Filled)-30% provides increased load bearing characteristics and is the choice.. |