Mechanical Properties Metric English Comments
Tensile Modulus 33.1 GPa
4800 ksi
MTI ThermoStran® PA66-30C Long Carbon Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Tensile Modulus 33.1 GPa
4800 ksi
0°; ASTM D3039
Polystrand ThermoPro™ IE7010 Unitape Unidirectional Polypropylene-Glass Composite
Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer ..