Mechanical Properties Metric English Comments
Tensile Modulus 32.0 GPa
4640 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RC008H PA 66
LNP THERMOCOMP* RC008H is a compound based on Nylon 66 resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare.
Tensile Modulus 32.0 GPa
4640 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON E9007E PEI
LNP* VERTON* E9007E is a compound based on Polyetherimide (PEI) containing 35% Long Carbon Fiber. Added features of this grade include: Structural, High Temperature
Tensile Modulus 32.0 GPa
4640 ksi
Hexcel® HexPly® ES 84 120°C Curing Epoxy Matrix, Aramid Balanced fabric 175 g/m2
Information provided by HexCel