Mechanical Properties Metric English Comments
Tensile Modulus 2.96 GPa
430 ksi
ASTM D638
Quantum PEI - Ultem®
Information provided by Quantum Advanced Engineering Plastics
Tensile Modulus 2.96 GPa
430 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Lubri-Tech™ ATH-000/2T Acetal-Homopolymer, PTFE Lubricated  (discontinued **)
Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation.
Tensile Modulus 2.96 GPa
430 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® PI-1000 Polyetherimide (PEI)  (discontinued **)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Tensile Modulus 2.96 GPa
430 ksi
ASTM D 638
Styrolution PS 1600 GPPS
Foam extrusion; Injection moldingGood balanced of strength, flow and heat resistanceFree of zinc and oil additivesInformation provided by Styrolution
Tensile Modulus 2.96 GPa
430 ksi
ASTM D 638
Styrolution PS 1900 GPPS
Foam extrusionVery high flowHigh heat resistanceFree of zinc and oil additivesInformation provided by Styrolution
Tensile Modulus 2.96 GPa
430 ksi
ASTM D638
Westlake Plastics Tempalux® Polyetherimide
An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad ..
Tensile Modulus 2.96 GPa
430 ksi
ASTM D638
Westlake Plastics Tempalux® Polyetherimide For Medical Applications
Medical grade Tempalux is made from Ultem® polyetherimide resin, an amorphous thermoplastic which exhibits excellent resistance to a wide range of chemicals and disinfectants. Ultem maintains its ..
Tensile Modulus 2.96 GPa
430 ksi
ASTM D638
Total PSC 585 Polystyrene
Polystyrene 585 is a high molecular weight, low melt flow, crystal polystyrene. This polymer is tailored for extruded foam applications such as egg cartons, meat trays and food service. 585 also mak..
Tensile Modulus 2.96 GPa
430 ksi
ASTM D638
American Polymers API 395 Polystyrene
API 395 is one of the highest flowing crystal polystyrenes commercially available. It is produced in pellet form for injection molding and compounding. This material is designed for hard to fill ..
Tensile Modulus 2.96 GPa

@Temperature 22.8 °C
430 ksi

@Temperature 73.0 °F
ASTM D638
Ensinger TECAPEI® made from Ultem® 1000 PEI
TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in..
Tensile Modulus 2.96 GPa
430 ksi
ASTM D-638
Axiall LR-5009 Rigid PVC, Molding, All Colors
Georgia Gulf LR-5009 is an economical high flow rigid PVC fittings compound designed for multi-cavity molds and large diameter fittings. This compound is characterized by excellent process ability,..
Tensile Modulus 2.96 GPa
430 ksi
ASTM D638
Asahi Kasei Thermylene® P6-10FG-0600 10% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Tensile Modulus 2.96 GPa
430 ksi
ASTM D638
Asahi Kasei Thermylene® P6-10FG-Y950 10% Glass Fiber Reinforced, Lubricated
Information provided by Asahi Thermofil
Tensile Modulus 2.96 GPa
430 ksi
ASTM D638
Amco Amalloy® B1044 Polymer Alloy
Amco Amalloy B1044 is a proprietary copolymer with exceptional clarity and toughness.Low haze, low melt flow, high tensile & flexural strength.Information provided by Amco Plastic Materials.