Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 341 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® 101 PC (Europe-Africa-Middle East)
LEXAN 101 is a high viscosity multi purpose grade available in transparent, translucent and opaque colours.
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® 103R PC (Europe-Africa-Middle East)
LEXAN 103R is a high viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 103R is available in transparent, translucent and opaque colours.
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® 164R PC (Europe-Africa-Middle East)
Medium viscosity, multi purpose polycarbonate resin with added release agent. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with b..
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® 201R PC (Europe-Africa-Middle East)
LEXAN 201R is a high viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved.
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® 2034 PC (Europe-Africa-Middle East)
LEXAN 2034 is a medium viscosity flame retardant grade. The material is UV-stabilized. Glow wire at 960C also satisfies EDF spec HN 60-S-02.
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific)
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER
Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an..
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co..
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® FXE101 PC (Europe-Africa-Middle East)
Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release.
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® IFX6420Z PC (Asia Pacific)
Lexan* IFX6420Z is a medium viscosity, release containing, injection moldable, polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grades meets the transm..
Tensile Modulus 2.35 GPa
341 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® IR1840 PC (Europe-Africa-Middle East)
IR1840 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® LI1911R PC
Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release.
Tensile Modulus 2.35 GPa
341 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® PC1800 PC (Europe-Africa-Middle East)
PC1800 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® VR2220 PC (Europe-Africa-Middle East)
VR2220 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East)
XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® 141R PC (Europe-Africa-Middle East)
LEXAN 141R is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 141R is available in transparent, translucent and opaque colours.
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® FXD163R PC (Europe-Africa-Middle East)
FXD163R is a Lexan PC Transparent grade in our VisualFX Portfolio. It is a light Diffusion effect, developed for today´s Aesthetic Differentiation Needs. Color package may effect properties, Ap..
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® HP4 PC
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mol..
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer
Transparent weatherable PC copolymer for blowmolding/extrusion.
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics PC0700 PC (Europe-Africa-Middle East)
PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T..
Tensile Modulus 2.35 GPa
341 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics PC0700 PC (Europe-Africa-Middle East)
PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It..
Tensile Modulus 2.35 GPa
341 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics PC1000 PC
PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r..
Tensile Modulus 2.35 GPa
341 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics PC1500 PC (Europe-Africa-Middle East)
PC1500 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East)
PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics PC2203R PC (Asia Pacific)
PC2203R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
Tensile Modulus 2.35 GPa
341 ksi
ASTM D638
Samsung Cheil Industries Starex® SF-0505H MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics PC1500 PC (Asia Pacific)
PC1500 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
Tensile Modulus 2.35 GPa
341 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics PC1803R PC (Europe-Africa-Middle East)
PC1803R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.