Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.07 GPa | 300 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | Type 1, .0125; ASTM D638 |
RedEye On Demand Polyphenylsulfone (PPSF), Rapid Prototyping Material Polyphenylsulfone (PPSF) is a durable high-end thermoplastic that can be used in the toughest applications. Parts built in PPSF can handle heat near 400°F (204°C), it resists petroleum products, a.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | 0.2 inches/minute; ASTM D 638 |
NOVA Chemicals Dylark® FG2500 High-Heat Styrenic Copolymer Product Description and Features: Styrenic copolymer with high-heat resistance, high-impact strength and good toughness. Resins used in food grade sheet extrusion and injection molding application.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM D 638 |
Styrolution PS 5801 HIPS Exceptional processabilityHigh toughnessUSP Class VI certifiedUl Classification 94 HBInformation provided by Styrolution |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM Data |
Styron Magnum™ 344CC ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | Type I, 51 mm/min; ASTM D638 |
Styron MAGNUMâ„¢ 347 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM D638 |
Total Impact Polystyrene 940E Super High Impact Polystyrene, Sheet Extrusion and Thermoforming Grade TOTAL Petrochemicals 940E is a super high impact polystyrene designed for high gloss sheet extrusion and thermoforming applications that require additional toughness.Applications: The combination o.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM D412 |
Clariant Renol TPU2072A Polyurethane Elastomer, Ether Based Data provided by Clariant Masterbatches |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | |
Plastcom SLOVALEN PH 61 GB 30 PP, 30% glass beads, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM Data |
Styron Magnum™ 4435 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM Data |
Styron Magnum™ 9020 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | blown films TD; ISO 527-3 |
Borealis Bormod™ HC904CF Polypropylene Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tech.. |