Polymer Property : Tensile Modulus = 2406 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 16.59 GPa
2406 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear
LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing 20% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Easy Molding, Electrically Conductive, Wear ..
Tensile Modulus 16.59 GPa
2406 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear (Asia Pacific)
LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Easy Molding.
Tensile Modulus 16.59 GPa
2406 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON OEL13I PPS - Linear
LNP* STAT-KON* OEL13I is a compound based on PPS-Linear resin containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: High Impact, Wear Resistant, Electrically Conductive.