Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 16.33 GPa | 2368 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66 LNP* LUBRICOMP* RCL34 is a compound based on Nylon 66 containing 20% Carbon Fiber, 15% PTFE. Added features of this grade includes: Wear Resistant, Electrically Conductive. |