Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.59 GPa | 231 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-000/10T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 1.59 - 1.66 GPa | 231 - 241 ksi | ASTM D638 |
Proto3000 Accura® 25 Plastic Stereolithography (SLA) Prototyping Polymer Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features: Look and feel of molded polypropyleneOutstanding feature resolution and accu.. |
|||
Tensile Modulus | 1.59 GPa | 231 ksi | ASTM Data |
Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified
(discontinued **) ISOPLAST® 151 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois.. |
|||
Tensile Modulus | 1.59 GPa | 231 ksi | 1mm/min |
Eastman Tenite 371A-12 CAP Cellulose Acetate Propionate
(discontinued **) 12% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Tensile Modulus | 1.59 GPa | 231 ksi | 1mm/min |
Eastman Tenite 264-10 CAB Cellulose Acetate Butyrate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Tensile Modulus | 1.59 GPa | 231 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic. |
|||
Tensile Modulus | 1.59 GPa | 231 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Tensile Modulus | 1.59 GPa | 231 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY K3000Z Acetal LNP* STAT-LOY* K3000Z is a compound based on unfilled Acetal resin. Added feature of this material is: Antistat. |
|||
Tensile Modulus | 1.59 - 1.66 GPa | 231 - 241 ksi | ASTM D638 |
3D Systems Accura® 25 Plastic for SLA® Systems For use with solid-state stereolithography (SLA®) systems.ApplicationsFunctional components for assemblies and mock-ups for:Automotive styling parts — trim, fascia, and other componentsConsumer el.. |