Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 15.13 GPa | 2194 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF00A8P PC (Asia Pacific) LNP* Thermocomp* DF00A8P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact perform.. |
|||
Tensile Modulus | 15.13 GPa | 2194 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP D551 PC (Asia Pacific) LNP* Thermocomp* D551 (or DF00A8P) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impa.. |