Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.47 GPa | 214 ksi | Storage |
Epoxy Technology EPO-TEK® EJ2189-LV Electrically Conductive Epoxy Low Viscosity, two component room temp curing conductive epoxyInformation Provided by Epoxy Technology |