Tensile Modulus 140 GPa
20300 ksi
Longitudinal tensile test (fiber direction)_These values are normalized to 60% of fiber volume fraction; ASTM D3039
Nanocyl EPOCYL™ NC R2HM-01 Formulated Epoxy-Carbon Nanotube Pre-preg Resin System
EPOCYL™ NC R2HM-01 is a formulated epoxy based resin system for hot melt pre-preg and pressure molding processes, modified with our own Carbon Nanotubes (CNT), specifically developed to enhance the..
Tensile Modulus 140 GPa
20300 ksi
Vf=59%
Toyobo Zylon® HM Fiber/Epoxy Matrix Unidirectional Composite
Poly(p-phenylene-2,6-benzobisoxazole) (PBO) is a rigid-rod isotropic crystal polymer. Zylon is a new high performance fiber developed by TOYOBO using the latest material science and state of the ar..
Tensile Modulus 140 GPa

@Temperature 23.0 °C
20300 ksi

@Temperature 73.4 °F
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix, Unidirectional Prepreg Laminate (M36/32%/135/HTA)
Tenax HTA fiberInformation provided by HexCel