Mechanical Properties Metric English Comments
Tensile Modulus 0.0138 GPa
2.00 ksi
TM R050-36
Resinlab® EP1121 Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP1121 Clear is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I..
Tensile Modulus 0.0138 GPa
2.00 ksi
500%; ASTM D412/D638
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission, good low temperature properties and elasticity.Uses: Blown and..
Tensile Modulus 0.0138 GPa

@Thickness 0.127 mm
2.00 ksi

@Thickness 0.00500 in
Cured; ASTM D638
Aptek DAT-A-THERM 1000 Electrically insulating urethane film
DAT-A-THERM 1000 is a tough, flexible, void free, electrically insulating urethane film designed to fill air gaps and dissipate heat between devices and substrates. DAT-A-THERM 1000 film is a 100% s..
Tensile Modulus 0.0138 GPa
2.00 ksi
Molded Properties; ASTM D638
ExxonMobil Escorene™ AD 2528EH2 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: AD 2528EH2 is a copolymer of ethylene and vinyl acetate. Availability: Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesFree Flowing Agent: Yes Applications:Hot Mel..
Tensile Modulus 0.0138 GPa
2.00 ksi
ASTM D1708
DuPont Elvax® 4355 Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® 4355 is an ethylene-vinyl acetate / acid terpolymer resin for use in industrial applications.ApplicationsElvax® 4355 resins can be used for the following applications: adhesives, s..
Tensile Modulus 0.0138 GPa
2.00 ksi
TM R050-36
Resinlab® EP1121 Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP1121 Black is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I..
Copyright © lookpolymers.com All Rights Reserved