Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.44 GPa | 1949 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Verton WV007XXP PBT (Europe-Africa-Middle East) LNP VERTON* WV007XXP is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |