Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.7 GPa | 1690 ksi | ASTM D638 |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Tensile Modulus | 11.65 GPa | 1690 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON EX99689C PEI LNP* STAT-KON* EX99689C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Tensile Modulus | 11.65 GPa | 1690 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp EC002E PEI LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas.. |
|||
Tensile Modulus | 11.65 GPa | 1690 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp EC002E PEI (Asia Pacific) LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Tensile Modulus | 11.65 GPa | 1690 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 11.65 GPa | 1690 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Asia Pacific) LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 11.65 GPa | 1690 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Europe-Africa-Middle East) LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |