Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 110 GPa | 16000 ksi | |
PSM Industries Pacific Sintered Metals Infiltrated High Carbon Steel FX-232-T Powdered Metal Good strength, shock resistance and hardenability, Moderate tolerance control Equivalent MPIF Specification: FX-1008-50Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
PSM Industries Pacific Sintered Metals Infiltrated High Carbon Steel FX-232-T(HT) Powdered Metal Good strength, shock resistance and hardenability, Moderate tolerance control Equivalent MPIF Specification: FX-1008-110HTInformation Provided by Pacific Sintered Metals, a division of PSM Industri.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
PSM Industries Pacific Sintered Metals Infiltrated Iron FX-226-T Powdered Metal Machines and plates well, Good in hydraulic applications, Moderate tolerance control Equivalent MPIF Specifications: FX-1000-25Information Provided by Pacific Sintered Metals, a division of PSM Ind.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
PSM Industries Pacific Sintered Metals Infiltrated Steel FX-227-T Powdered Metal Machines and plates well, Good in hydraulic applications, Moderate tolerance control Equivalent MPIF Specifications: FX-1005-50Information Provided by Pacific Sintered Metals, a division of PSM Ind.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 240 Low Brass, 1/4 Hard CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 240 Low Brass, 3/4 Hard CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 240 Low Brass, Extra Hard CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 260 Cartridge Brass, Annealed Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 260 Cartridge Brass, Extra Spring Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 425 Tin Brass 2%, 1/4 Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 425 Tin Brass 2%, Annealed Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 425 Tin Brass 2%, Extra Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 425 Tin Brass 2%, Spring Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 510 Phosphor Bronzes 5% A, 3/4 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 510 Phosphor Bronzes 5% A, Annealed Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 510 Phosphor Bronzes 5% A, Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 511 Phosphor Bronzes 4%, 1/2 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 511 Phosphor Bronzes 4%, 1/4 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 511 Phosphor Bronzes 4%, 3/4 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 511 Phosphor Bronzes 4%, Annealed 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 511 Phosphor Bronzes 4%, Extra Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 511 Phosphor Bronzes 4%, Extra Spring 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 511 Phosphor Bronzes 4%, Spring 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 521 Phosphor Bronzes 8% C, 1/2 Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 521 Phosphor Bronzes 8% C, 1/4 Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Spring Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Modulus | 110 GPa | 16000 ksi | |
Eagle Brass 521 Phosphor Bronzes 8% C, Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Modulus | 110 - 120 GPa | 16000 - 17400 ksi | Longitudinal |
Goodfellow Carbon/Epoxy Composite Tube Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |